Customization: | Available |
---|---|
After-sales Service: | Free Spare Parts, Field Installation, Commissioni |
Warranty: | 2 Years |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Precast concrete elements: Piles, wall panels, railway sleepers, etc. Steam curing reduces demolding time to 8-12 hours (compared to over 7 days for natural curing).
Fiber cement boards: Such as calcium silicate boards and GRC (glass fiber-reinforced cement), where steam curing enhances early strength.
Foamed concrete: Steam improves foam stability and uniformity.
Polymer-modified cement composites: Steam assists in resin cross-linking (e.g., epoxy cement).
Recycled aggregate activation: Steam treatment enhances the bonding properties of waste concrete aggregates.
Building materials industry: Drying and hardening of gypsum boards and lightweight aggregate panels.
Eco-friendly materials: Solidification of industrial waste (e.g., fly ash bricks).
Temperature control: Avoid rapid heating to prevent microcracks (recommended rate ≤20°C/h).
Humidity requirement: Maintain >95% relative humidity to prevent moisture loss.
Curing cycle: Typically includes pre-curing (room temperature), heating, constant temperature (2-8 hours), and cooling phases.
Item | ETSA-RA800 | ETSA-RA1200 | ETSA-RA1500 | ETSA-RA1700 | ETSA-RA2000 | ETSA-RA2600 |
Inner diameter(mm) | 800 | 1200 | 1500 | 1700 | 2000 | 2600 |
Canister length(mm) | 22000 | 3000 | 3000 | 4000 | 5000 | 10000 |
Number of lid sawtooth | 12 | 12 | 14 | 14 | 16 | 24 |
thickness of lid (mm) | 10 | 10 | 10 | 10 | 16 | 14 |
Thickness of the tank body(mm) | 10 | 10 | 10 | 10 | 12 | 14 |
Working pressure(Mpa) | 0.8 | 0.8 | 0.8 | 0.8 | 0.8 | 0.55 |
Dimensions(mm)(L*W*H) | 22766*1445*1170 | 4010*1575*1670 | 3960*2150*2050 | 4925*2162*2070 | 6200*2590*2424 | 11722*3360*4136 |
Weight(Kg) | 5580 | 2017 | 2950 | 3835 | 6500 | 16775 |